1.7mm Flexographic printing plate
1. Item: 1.7mm Flexographic printing plate
2. Description:
3)Excellent dot and isolated line reproduction
4)Solid printing performance
5)High latitude of exposure and processing
6)Good ink transfer
7)High impression.
3-Technique Data and information for your reference:
Type | R-394 | R-284 | R-228 | R-170A | |
Thickness(mm) | 3.94mm | 2.84mm | 2.28mm | 1.70mm | |
Rigidity(Shore A) | 38-45 | 50±2,60±2 | 53-56 | 60±2,67±2 | |
Recommend relief depth(mm) | 1.8-2.0 | 1.0-1.2 | 1.0-1.1 | 0.7-0.9 | |
Image reproduction | 5%~95% | 2%~95% | 2%~95% | 2%~98% | |
Maximum line line/inch | 100 | 120 | 133 | 150 | |
Minimum isolated line | 0.3mm | 0.175mm | 0.10mm | 0.10mm | |
Minimum isolated dot | 0.50mm | 0.25mm | 0.15mm | 0.15mm | |
Suitable ink | Suitable for water and alcohol-based ink, incompatible with oil-based ink, hydrocarbon solvent or the ink containing ethyl acetate of more than 25% | ||||
Mainly applicable field | Corrugated board, thick board | Corrugated board, thick board | Label, flexible package, carry bag, folded paper box and beverage package | Film, label, flexible package, carry bag, folded paper box | |
Storage—raw plates | Unexposed plates should be stored in cool areas (4-32°C)away from heat. The plates must be placed flatly, and protected from contacting UV light. It is recommended to unpacked and handled in yellow light. | ||||
Storage—finished Plates | Printing plate should be avoid excessive white light, irradiating from sunlight and exposing in high concentrated ozone environments for a long time either. After being unloaded, the plates should be cleaned thoroughly. | ||||
Guarantee Period | Under the recommended storage condition, guarantee period of Flexographic Printing Plate is 12 months. | ||||
Packing | 60"*30"(1524mm*762mm), 8 pcs/ctn40"*30"(1016mm*762mm), 8 pcs/ctn42"*60"(1067mm*1524mm), 8 pcs/ctn | 80"*50"(2032mm*1270mm), 6 pcs/ctn | 80"*50"(2032mm*1278mm), 10 pcs/ctn | ||
4.Processing of Photopolymer flexo plate:
Type | R-394 | R-284 | R-228 | R-170A |
Thickness( mm) | 3.94 | 2.84 | 2.28 | 1.70 |
Back exposure(seconds) | 20-60 | 20-40 | 20-40 | 30-80 |
Main exposure(minutes) | 5-20 | 5-20 | 8-20 | 8-20 |
Rinsing(minutes) | 5-7 | 5-7 | 5-7 | 5-7 |
Minimum drying time(hourrs) | 1.5-2 | 1.5-2 | 1.5-2 | 1.5-2 |
Detackfying(minutes)) | 8-15 | 8-15 | 8-15 | 8-15 |
Post exposure(minutes) | 5 | 5 | 5 | 5 |
5.Packing
6- Please check the process of placing an order
1-Please kindly send us your professional inquiry. | ||||||||
2-We will send you our professional quotation with price, packing, technique data and company information. | ||||||||
3-Confirming the price, lead time, payment or some artwork. | ||||||||
4-We will send some samples for your test. | ||||||||
5-When quality is approved, clients confirm quantity, then we make commercial invoice. | ||||||||
6-Clients pay the deposit and send us the bank receipt. | ||||||||
7-We start production according to clients' requirement. | ||||||||
8-We communicate with clients about the progress of production. | ||||||||
9-We take photos when production finished, clients pay the balance by T/T or by L/C. | ||||||||
10-Order can be say “finish” when you receive the goods and satisfy with them . | ||||||||
11- Feedback to Freedom about Quality , Service, Market Feedback & Suggestion. And we can do better . |
Please feel free to contact me online or send me a message if you are interested in our products, thank you!
Contact person: Alice Zhou
Cell phone: 0086-18662520095
1.7mm Flexographic printing plate